Re: [MW:30322] Filler material Selection

Received clarification from the client about using E316L to weld Carbon steel.
Their welders are qualified to weld steel (P1 to P15) with filler material (F1 to F4).
They want these welder to be qualified for F No. 5 but do not have austenitic steel base metal in stock. Only Carbon steel is available in stock.
Therefore, they have requested a PQR to weld Carbon steel base metal P No 1 with E316L and ER 316L (F5 and F6).
In case the coupon meets ASME Section IX Nondestructive and destructive testing requirements, they will prepare a WPS which shall be used only to qualify welders for F number.

On another note, I hope to receive guidance on selection of filler materials in general. 
What are the parameters to be considered to select filler materials for any base metal and whether it is addressed by general standards in the industry.

Thanks and best regards,
Navanith




On Tue, 24 Dec 2019 at 06:08, HENNING John <John.Henning@hamon.com> wrote:

Possible, yes, but not for Section I if water wetted service.

 

Practical, no, absolutely not.  I have a really difficult time trying to come with any reason to do this and a host of possible issues if done.

 

Enjoy - John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Navanith
Sent: Sunday, December 22, 2019 6:26 AM
To: Materials & Welding
Subject: [MW:30305] Filler material Selection

 

Dear Experts,

 

Require guidance on filler material selection as per ASME BPVC.

For example:I received this query from a client

Base metal is ASTM A106 Gr.B and they want to weld using E316L electrodes.

Is it possible to use E316L electrodes to weld directly?

 

Regards,

Navanith

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/37bac14e-c9a8-4d35-af83-c5e116da3bc8%40googlegroups.com.

DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/AM6PR0102MB32395B8DBC0BC94451EA395C902E0%40AM6PR0102MB3239.eurprd01.prod.exchangelabs.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9p%2B5ruv%3DqFnfWTgqJzJaG6S-HNm2UhyDjFN%2B9zbGUv3WxCNw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...