Possible, yes, but not for Section I if water wetted service.

 

Practical, no, absolutely not.  I have a really difficult time trying to come with any reason to do this and a host of possible issues if done.

 

Enjoy - John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Navanith
Sent: Sunday, December 22, 2019 6:26 AM
To: Materials & Welding
Subject: [MW:30305] Filler material Selection

 

Dear Experts,

 

Require guidance on filler material selection as per ASME BPVC.

For example:I received this query from a client

Base metal is ASTM A106 Gr.B and they want to weld using E316L electrodes.

Is it possible to use E316L electrodes to weld directly?

 

Regards,

Navanith

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/37bac14e-c9a8-4d35-af83-c5e116da3bc8%40googlegroups.com.

DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...