Re: [MW:30307] Filler material Selection

Use 309

On Mon, 23 Dec 2019 10:55 am Navanith, <navanitheeshwaran@gmail.com> wrote:
Dear Experts,

Require guidance on filler material selection as per ASME BPVC.
For example:I received this query from a client
Base metal is ASTM A106 Gr.B and they want to weld using E316L electrodes.
Is it possible to use E316L electrodes to weld directly?

Regards,
Navanith

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/37bac14e-c9a8-4d35-af83-c5e116da3bc8%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOoo2%2BtTAVKLFOFkG%2BHHkyYUkbUqZ1GZCWuQ84hJkrA2A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...