Re: [MW:30290] Minor Cracks in SAW Welds Cap

Mr.Rishikesh Kumar &  Raghuram Bathula,

Material - S355ML
Thickness - 40 mm  
Consumable - F7A8-EM12K
Process - SAW ( Tandem)
Heat Input - 3.15 Kj/mm
Preheat - Not applicable
Post heat - Not applicable


On Tue, 17 Dec 2019 at 11:32, Rishikesh Kumar <rishikr06@gmail.com> wrote:
Can your share more information  like material, consumable, welding process and sequence, heat input,etc . then anybody might help in right direction...


On Tue, Dec 17, 2019 at 11:28 AM Gowtham Rajendran <rajgowthamiwe@gmail.com> wrote:
Dear All,

In the cap pass of the SAW Welding, we have observed some minor cracks while performing MPI as you can find in the attached pics.

With pipes welded with the same parameters and almost the same condition, we are finding this kind of defect in some pipes, if anyone has come across such kind of defects, kindly share your experience and possible root cause.

Thanks in advance for your valuable inputs.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABLAf1L-TDhOLG1vDXgLLrvZOA2wW3dj-gqwk6dLTvhAdM%3DRuA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEXs1Ko%3D0OAR353SM%3DPic5sgpvT8cFHzVhq3Fw3-mkBSE_SZjw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABLAf1LNmmwYMZG-CDejZ6Ni5h-p-zfgFczeGKXz%2Bsy%2B0s0hCg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...