Re: [MW:30285] Re: Hard Facing Overlay Test Required

What you have welded is not a Corrosion Resistance overlap, it is a Hardsurfacing overlap, in which no PRN required. Only Hardness value is required. Thanks

On Tue, 17 Dec 2019 8:54 am raghul k, <raghul351991@gmail.com> wrote:
HI,
        Actually when i worked in Aramco project,They recommended min PREN value for overlay portion as per SAES.

common formula for PREN value=%cr+3.3 X Mo%+16 x N%

           

On Mon, Dec 16, 2019 at 3:13 PM sathish <qms.pjgpl@gmail.com> wrote:
Dear Mr.Ragul
Thanks for the response.

How to ensure that PREN meeting the chemical analysis. I have tested Welding of ERCoCr-A PTAW powder with ASTM A36, SS316L, F11,F22,F91 MATERIALS.

 Can you provide which standard or value to refer for acceptance and how to check the same?


Regards
S.Sathish kumar

On Thursday, 23 May 2013 02:03:26 UTC+5:30, Biplab Pal wrote:
Dear Experts,

Please give me the guide for Hard facing Overlay:
We did a) Visual Examination, b) LPT, c) Hardness Test, d) Macro, e)
Weld Metal chemical analysis.
Is there any other mechanical or other test required for HFO like
Tensile or Bend test required?
Please guide me with ASME Sec IX 2010.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com

Information in this email and any attachments is confidential and intended
solely for the use of the individual(s) to whom it is addressed or
otherwise directed. Please note that any views or opinions presented in
this email are solely those of the author and do not necessarily represent
those of the Company. Finally, the recipient should check this email and
any attachments for the presence of viruses. Myself accepts no liability
for any damage caused by any virus transmitted by this email.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/88bade01-a7a9-4aef-8bc4-b24df34abf4f%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC69MwCP7yWVPDw-0tsZc4G8u7_Wp4xdntnjKkLvs_teud_YyQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePTDNiW47ejRK3zLfOg6F7os2xjkdQsCk-JOPSw30sHRg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...