Re: [MW:30281] PQR shall be tested in Min & Max PWHT (3 Cycle minimum simulation) condition.

What is your governing thickness.?

Also specify design code.

Thank you 

Vijay Katkar 


On Mon, 16 Dec 2019, 1:56 pm , <kunalenfield350@gmail.com> wrote:
Dear Sir's

Client has specified the requirement for testing the PQR in Min & Max PWHT (3 Cycle simulation) condition. As we had pre-qualified PQR with one cycle of 2 Hours soaking. So please suggest how to comply with the requirement & what does this "3 cycle simulation" exactly means?


Regards
Kunal Srivastava

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3a501189-a776-4557-a36c-bfdc41b280bb%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wr%2BjiJn6UjF0SYtV8w9F%2BXBzjt%3D3s0vbqHUq5CiANi4N9w%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...