Dear sathish,

              On overlay.chemical analysis will be related to PREN (Pitting resistance equivalent number) not to asme sec II part C.

On Mon, Dec 16, 2019 at 7:09 AM sathish <qms.pjgpl@gmail.com> wrote:
Dear Expert
As i have weld deposit to 4-5mm ERCoCr-A on Astm A36 and 1.6mm finished thick of weld metal from base metal.
1. on 1.6mm I have made chemical analysis, my doubt is that did i need to verify the element of chemical avilable for ERCoCr-A filler wire from ASME Sec II Part-C.

If i check Fe value is not meeting to Filler wire, As the Base metal having Fe about >98% and filler wire 3% on dilution and taking test at 1.6mm it is not achievable.

Kindly suggest some inputs on this requirement


Regards
S.Sathish kumar 

On Thursday, 23 May 2013 02:03:26 UTC+5:30, Biplab Pal wrote:
Dear Experts,

Please give me the guide for Hard facing Overlay:
We did a) Visual Examination, b) LPT, c) Hardness Test, d) Macro, e)
Weld Metal chemical analysis.
Is there any other mechanical or other test required for HFO like
Tensile or Bend test required?
Please guide me with ASME Sec IX 2010.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com

Information in this email and any attachments is confidential and intended
solely for the use of the individual(s) to whom it is addressed or
otherwise directed. Please note that any views or opinions presented in
this email are solely those of the author and do not necessarily represent
those of the Company. Finally, the recipient should check this email and
any attachments for the presence of viruses. Myself accepts no liability
for any damage caused by any virus transmitted by this email.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/483f1f8d-925d-4436-8f09-5eb3dc2a363c%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC69MwCD6w5KPaVRsCMkBHboojXdgwB6-EHHsjMS1H%3DG-sL78g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...