Re: [MW:30267] Selection of 10%weld joints of pipeline

Totally agree with Mr. Balajirajan's reply.
10% of each welder and total 10% of all the welds. If you have some welds at shop and some at field than choose field joints for radiography test.

Thanks & Regards
Atul Khatri

On Mon, Dec 9, 2019 at 9:40 AM Balajirajan Palanisamy <pbrerode@gmail.com> wrote:
Dear Akash,
   You need to select 10% of complete joint RT in total number of joints. i.e 1 joint per 10 joints.

Normal practice, If you have more than one welder, then 10% of joints you should select from the number of welds did by that welder, as that you can cover 10% RT for that line class and also for the welders. By this you can come to know the integrity of weld and also the welder performance.

On Sat, Dec 7, 2019 at 8:40 AM Aakash <harenathjha@gmail.com> wrote:
Hello expert ,
We are having 10% RT, pipe size is 16inch, please suggest should I select one complete joint or one segment of all the joints. Please provide the codal reference if any ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/01379daa-22dd-4bfd-ae0b-335e77f9e8d5%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEXdmd9JYVwQL6%3D_MsitS_erVEVc%3DDQC%2Be7-TuOFhUzN00kybQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeABY9xoE3xcaCYgSCw%2BhHBafU9Du3zqS7Pkuq8sT1KG4Q%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...