Wednesday, December 4, 2019

Re: [MW:30254] WPS of HOT TAPPING

Dear Friend,

please refer article 10, section 4.1.1 in ASME PCC-2 Ed:2015.

Regards 

NOUFAL MC


On Wed, Dec 4, 2019 at 11:55 AM <asgharialigl@gmail.com> wrote:
Dear All.

If we want to qualify a WPS for hot tapping on pipeline, we shall apply Appendix B of API1104.
But for hot tapping of piping section for qualification of WPS, which code have to be applied, with regard to ASME IX doesn't mention to in service welding?

Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1f432d89-8224-49ba-a8f0-fb716bf6a663%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BnmLwVmTCeci%2B-wRtHBV9MLQ0tMeKSfTTRB8%3DGdeNAoy0T0jw%40mail.gmail.com.