Re: [MW:30248] Time lag between Hydro test Dewatering completion and swabbing completion

Thanks for your update.
My concern is time lag between Dewatering to swabbing activity

On Tue, 3 Dec 2019, 09:35 Noufal Mc, <noufalmc.mc@gmail.com> wrote:
Pradip,

As per ADNOC specification De watering should be completed within one week. please see below snapshot extracted from DGS 9550-002 rev 1.



regards 

NOUFAL MC

On Mon, Dec 2, 2019 at 1:24 PM pradip kumar Sil <pradipsil@gmail.com> wrote:
Dear All,
Can anybody inform me How much  time lag between Hydro test Dewatering completion and swabbing completion in the pipeline with code reference.
Regards
Pradip

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DdXk%2BFh7JXe-062dsyd6c0_2%2BSGaSusbbgGPyBPFymcA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BnmLwURejWiv_pATP%2B__FFjDjgyM%3DEbow69X%2B4_eG50dHzL0w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8n0JKSaZJNDYFurEh7bpsAm1dmm48dTd8AjE_gQsAQLBA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...