Thursday, December 19, 2019

[MW:30295] Preheat temperature of EN10025 S 275 JR and S355JR

Dear Experts,

I have to weld S275 JR and S355JR  of unlimited thickness as per AWS D1.1 but the material are unlisted material.  In Table 4.9 the unlisted material preheat temperature is not shown but in WPS what temperature I should provide and on what basis.

Thanks in advance

Manoj,
Welding Inspector.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5nJDi7gOCwBAP407QNfe011tzX4PsxJdpwD69b9jgPqsg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...