Saturday, October 26, 2019

Re: [MW:30186] WPS /PQR Approvel

If Lab is authorized by national, international (ISO/IEC 17025) or by the Client, you can review the parameters and you can approve.You should have adjustment there is no malpractice have done by both of them. You can also review any past experience with the lab and you can also go and witness the lab calibrations and qualifications, if everything OK then only you can make an NC for why there is communication gap happened? otherwise you can not reject the WPS unless there is any one suitable reason.

Just my opinion.

Best Regards,

Venkat. G

On Fri, Oct 18, 2019 at 2:38 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
is vendor stamp holder

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Oct 18, 2019 at 4:59 PM Dinesh Somwanshi <som.din@gmail.com> wrote:
Dear sir, 

If it's NABL approved lab in India,  may consider for approval. 

For EIL approved jobs, May not possible to approve. 

Applicable to Indian client works only. 

Regards

Dinesh

On Fri, Oct 18, 2019, 16:32 Santosh Patil <raj.san23@gmail.com> wrote:
Dear Members 


I have witnessed PQR of  SA312 TP 316 material 1" SCH 40  according to  Proposal WPS  , Test piece visually checked and send to Lab for check testing as per. Sec IX . also inform to vendor to be witness in Lab in the  presence of QC engineer . 
But vendor does not infirm to QC Engineer . and Lab test report is submitted . Now he pressurizes to approve WPS 
What shall I do..... 
S. B Patil

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAETO-3tBgdsVjUKbeb6BcAFMP%3DkuaPkErfTXe76vYDtxP_O%2BFw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrXjhfFL4PmvyOMf4uKJ10n%3Dt-6Ls%2Byg06%3DAnxk%2BQOyLhA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePPLR8e42WcWTS1t5XAwXDJcykP1z2mo--Ygw1HrszmhA%40mail.gmail.com.


--
Venkatachalam Govindan
QHSE Lead / Trainer
(IRCA Registered Lead Auditor & API / CQI Practitioner)
+965 97604989, +919840502376 (
WhatsApp only)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHOK3OfGoo7miDQVv28A6SWx-iC6qBBroUao2zuwWg_zaw7w_A%40mail.gmail.com.

No comments:

[MW:35742] PQR- Chemical testing requirements

Good Day to all, Reference std: ASME SEX IX Material ASTM A106 Gr B Pipe Dia and thickness: 2" and 8.74 mm. Service Fluid: Normal fluid...