if welding is done to form dish end ( like Pettal construction) then ur pqr should under all heat treatment.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Wed, Oct 9, 2019 at 11:48 AM sandeep kumar <sandeepdhiman63@gmail.com> wrote:
Refer ASME Section IX, QW 407.1 as your dishend are single piece and will be normalized before welding. So you have to follow PWHT for qualification which is applicable after welding for your vessel.--
On Monday, August 12, 2019 at 1:14:19 PM UTC+3, chiluka venkatramulu wrote:Dear All,Pl clarify the below.One of vessel under fabrication will under go the fallowing heat treatments. (Material-516 G 70, shell-63 mm, dish end -75mm, dish end in one piece only)
- Dishends Normalising-2 cycle.
- PWHT for whole vessel.
Now shall I need to do all three heat treatment cycles to qualify WPS?OROnly two normalising cycles are enough?Regards,Venkatramulu
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6f573a01-0566-416e-99fa-248437a11066%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM_X0p0ZcV5NKAaz1HbOadrwL3j%2BVc%3DLkQtdsYKA9ntJw%40mail.gmail.com.
Comments