Re: [MW:30106] RE: MATERIAL SPECIFICATION

It's a typo error. Just confirm with client if need to go with SA965 F 316L or any low alloy grade from SA 336.

On Oct 1, 2019 1:45 PM, "VIshal Suthar" <vishalsuthar3017@gmail.com> wrote:
Dear Members,

Please note one of equipment client specification mentioned Tubesheet material SA 336 F 316L.

Reference to ASME Sec-II Part A SA336 is for Alloy Steel Forging which not having 316L.

Please provide your valued suggestion.

Regards,
VIshaL SUTHAR

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOZ%2B%2BqCknkahgMMvgfnX_KZs02j5MOZ_uppOzVPPyiK96uRoJA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMVxSipu9X0NyvUSpSyiZfQpbJeiP-GkCzNRtthL24--7AxuTg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...