Sunday, October 6, 2019

Re: Atención valide origen![MW:30117] Distance between two weld joint

Good info

On Fri 4 Oct, 2019, 5:03 PM Hernan Arturo Castillo Mier, <Hernan.Castillo@ecopetrol.com.co> wrote:

Hello:

 

 

 

 

 

 

 

Hernán Castillo Mier

Ingeniero Senior Confiabilidad e Integridad

FACILITADOR AUTORIDAD TÉCNICA EQUIPO ESTÁTICO

INSPECTOR AUTORIZADO

API 510 (33119)

Avantel: 8*1571

Teléfono: 668-2396

 

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de siva Guru
Enviado el: viernes, 4 de octubre de 2019 6:18 AM
Para: materials-welding@googlegroups.com
Asunto: Atención valide origen![MW:30113] Distance between two weld joint

 

Dear All

Can you advice, 

two weld  joint how much Min distance between weldjoints.

Please clarify, if possible please provide code reference.

 

Best regards

 

Guru

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEDN%2BXFp1f7duhV4NFBmu_87QNzsuA877q4wDUTDuEOPTOM7eQ%40mail.gmail.com.

Este mensaje puede contener información de tipo personal, clasificada o reservada; si usted no es el destinario, por favor, hacer caso omiso de su contenido y abstenerse de compartirlo, reenviarlo o copiarlo. Si recibe este mensaje por error, agradecemos informarlo inmediatamente al remitente y borrarlo permanentemente de su cuenta. Si usted está autorizado para recibir la información de tipo personal, se le recuerda que esta información debe ser manejada con la finalidad con la que ha sido solicitada y en virtud de la normativa que habilita el acceso a la misma. Así mismo, deberá ser usada bajo los parámetros de la ley 1581 de 2012 de protección de datos personales y la normativa que la desarrolla, siendo responsabilidad del área receptora del cumplimiento de la citada normativa de protección de datos personales. CONFIDENTIALITY NOTICE: This electronic transmission (including any files attached hereto) (this "Communication") contains information that is or may be legally privileged, confidential, and exempt from disclosure without our express permission in advance. The information is intended only for the use of the individual or entity named above. If the reader of this message is not the intended recipient or any employee or agent responsible for delivering the message to the intended recipient, you are hereby notified that any disclosure, dissemination, copying, distribution, or the taking of any action in reliance on the contents of this electronic Communication is strictly prohibited. If you have received this Communication in error, please notify the sender immediately and destroy permanently the transmitted information in its entirety and do not disclose its contents to any other person. Para conocer la Declaración de Tratamiento de Datos Personales de Ecopetrol, favor consultarla en www.ecopetrol.com.co Responsabilidad Corporativa – Declaración de Tratamiento de Datos Personales.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BN6PR2201MB1092167BC6C7B21E37C4CC6DDD9E0%40BN6PR2201MB1092.namprd22.prod.outlook.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKBH9tOT_F28WcG27HYYBRYy%2Bnkvff0Lsi2_%2BY1VV3uKSyQrKA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...