On Friday, 25 October 2019 11:05:05 UTC+5:30, Bhima Kanjariya wrote:
-- if possible please provide party contact who expert in doing Al welding
On Friday, 25 October 2019 11:05:05 UTC+5:30, Bhima Kanjariya wrote:
hello friendsWe have one aluminium alloy Bucket used in Urea Prilling tower (pics attached for reference)We found a through crack in T-joint fillet welding of two plateplease advise how to weld and also suggest party who expert in welding aluminiumThanks in AdvanceBhima Kanjariya