Re: [MW:29533] REG : HARDFACING(ST-6) PRECAUTIONS OVER Cn3Mn CASTINGS


If you use Chromium carbide base welding consumable for Abrasion Resistance then crack is Natural, Deposit max 2 Layer ( 6 to 8 mm )

With Regards


Rahul J Rathod 
Welding Technician 

mob +91 9727076573

whats up +91 81155889118

 view my profile onLinkedIn view my profile on facebook my skype id


On Mon, 29 Apr 2019 at 19:04, RAHUL Rathod <welder.tigarc6g@gmail.com> wrote:
Dear Venkatesan 

Can you tell me what is your work Application, as per my knowledge some welding consumables have a natural tendency to crack due to high hardness if the crack is transverse, then no problem & please tell me which welding consumable you use & how much hardness its give as welded?
  

With Regards


Rahul J Rathod 
Welding Technician 

mob +91 9727076573

whats up +91 81155889118

 view my profile onLinkedIn view my profile on facebook my skype id


On Mon, 29 Apr 2019 at 12:47, <srimasstech@gmail.com> wrote:
DEAR EXPERTS 
                               WHILE HARDFACING DONE IN PTA WELDING OVER CN3MN MATERIAL WE FOUND SMALL (3-4 MM LENGTH) CRACKS IN EVERY WHERE.PLEASE GUIDE US WHAT ARE ALL THE PRECAUTIONS WE CAN MADE BEFORE WELDING ?

REGARD'S
M.VENKATESAN
SRIMASSTECH 
CHENNAI

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...