All the below combinations can be written as per the qualified pqr, if no change in F no.

Regards
Muneeb

On Sun, Apr 28, 2019, 8:21 PM Souravbohray <ermechsouravbohray@gmail.com wrote:
1.p number is essential variable  either impact required or not .
2.g number is essential impact required 
3.f and a number is essential  either impact required or not
so we can only weld P-No. 1 Gr. No 2  to  P-No.8 Gr.No.1
CORRECT ME IF I AM WRONG

On Monday, 24 August 2009 09:27:51 UTC+5:30, Kural wrote:
Interpretation: Answer is yes ( for all 3 combination of basemetals) as long as other essential and supplemtary essential are unchanged.
 


 
On Sun, Aug 23, 2009 at 9:48 PM, Sukamal Naskar <sukama...@gmail.com> wrote:
Dear All,
Good Morning !!!
 
I have a query on ASME SEC-IX ( 2007 ED, 08 ADD )
 

QW-403.5 (c ) , states that " ---------------   In addition, when base metals of two different P-Number Group Number combinations are qualified using a single test coupon, that coupon qualifies the welding of those two P-Number Group Numbers to themselves as well as to each other using the variables qualified."

 

Query: If we qualify one PQR, with P-No. 1 Gr. No 2  to  P-No.8 Gr.No.1 material using  SMAW ( E 309MoL) process with impact testing  on weld metal & both HAZ portion , does this PQR supports the following WPS combination of base metals , if all other welding variables are unchanged ?

 

(i)                  P-No. 1 Gr.No.2  to  P-No. 1 Gr.No.2 

(ii)                P-No. 1 Gr.No.2  to  P-No. 8 Gr.No.1 

(iii)               P-No. 8 Gr.No.1  to  P-No. 8 Gr.No.1 

 

Please give your comments,

 

Thanking you,

Regards,
--
Sukamal Naskar
Malaysia





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...