Re: [MW:29521] SAES W-12 PARA 6.1.5 NEED A CLEAR EXPLANATION

Standard clearly says cellulosic electrode may be used up to x60. So you cannot weld x65 with cellulosic. But if satisfying the requirements through pqr , no problem to weld with it.

On Sun 21 Apr, 2019, 6:58 PM Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
Cellulose has got 30 to 60 ppm of Hydrogen. It is better not to use in high strength steel and thickness

On Sun, 21 Apr 2019 5:44 pm Akhil, <AKHILSUNDAR.NBC@gmail.com> wrote:
Hii



IN SAES W 12 , PARA 6.1.5  It is mentioned that cellulosic electrode may be used for all passes of grith weld of grades upto and including x60 and wall thickness less than or equal to 25 mm. Is this a mandatory requirement for doing pqr IN aramco project, if i want to use cellulosic electrode in all passes(E-7010 P1  for root & E-8010 P1 for all other passes ) of grith weld of x65 pipe is it possible ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...