Re: [MW:29520] Inconel 825 - Corrosion Test for PQR

IGC is required as per MESC SPE 77 302.


Best Regards,
 
Abdul Rauf  
Abu-Dhabi UAE


On Sat, Apr 27, 2019 at 6:25 AM Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:
Dear all,

What kind of Corrosion Test can be suggested to Client for Inconel 825, if no specific corrosion test is mentioned in Spec.?

MOC - Inconel 825
Design Temp - 158 ℃
Service - H2S + Chlorine environment

Regards,


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...