Thursday, April 11, 2019

Re: [MW:29487] ASTM A106 Gr B to EN8

Dear Mr.Kadir,
You can use ER 70S-6 wire spool for welding of described MOC.
Ensure minimum preheating required for EN8 according to CE value.

Best Regards,
Darshan Revdiwala  

On Thu, 11 Apr 2019, 9:28 am , <kadirgodil@gmail.com> wrote:
Dear experts,
i require to chose filler metal for MIG welding of ASTM A106 gr b pipe with EN8 rod.
please help me which filler metal should i go for.

BR
A Godil

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...