What's the application?

·         Refinery, if so what units

·         Petrochemicals

·         Offshore O&G processing

 

Required  corrosion tests could differ a lot based on the service environment. However  you may take look at the attached data sheet and conclude what's the best to be recommended to  your client. The highlighted tests may be of relevance.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Hrushikesh Sangamnerkar
Sent: April 26, 2019 9:12 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:29515] Inconel 825 - Corrosion Test for PQR

 

Dear all,

 

What kind of Corrosion Test can be suggested to Client for Inconel 825, if no specific corrosion test is mentioned in Spec.?

 

MOC - Inconel 825

Design Temp - 158 ℃

Service - H2S + Chlorine environment

 

Regards,

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...