Monday, April 8, 2019

[MW:29475] EQT FOR SFA 5.9M

Dear Gents,

We have to do EQT for E 308L in our project, my question is how to
prepare test piece. In ASME SEC IIC we don't see any figure for test
piece preparation. Please advice us,

Thanks in advance.

Thanks & Regards

N.Kiran kumar,