Re: [MW:29011] Tube to Tubesheet Mock up Test

required when your project specification asks  for...

On Wed, 30 Jan 2019 at 15:02, chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:
Dear All,
Pl clarify, when the Tube to Tubesheet Mock up Test is required. Is it required when specific material combinations are there? or  for all Tube to Tubesheet welds? Give code reference pl.

Regards,
Venkatramulu


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...