Re: [MW:28997] Use of ss309 electrode in cracked area

If you want to draft a nice repair procedure refer to NBIC part 3. If you want to spend money use a nickel based electrode unless you are in a strange chemical environment 

Στις Παρ, 28 Δεκ 2018, 14:13 ο χρήστης Gopalakrishnan G <gopal2408@gmail.com> έγραψε:
Dear experts
Whether it is advisable to use ss309 electrode to arrest the crack in mild steel material .As my job is fully machined it is difficult to completely remove the crack.kindly guide me.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...