Saturday, January 26, 2019

Re: [MW:28979] SB-209 Grade 5183-PQR failure

First of all, tell me where the failure happened ?! Is it in the base metal or HAZ or weld metal ?! 


Thanks and regards
Hisham Almetwally
QC Engineer & Welding Engineer
Mob: +971564337326 & +971526679935

On Sat, 26 Jan 2019, 11:17 am Himan Nikdin <himan.nikdin@outlook.com wrote:
Boxbe This message is eligible for Automatic Cleanup! (himan.nikdin@outlook.com) Add cleanup rule | More info
RT done, some porosity observed, but in the acceptable critera per ASME IX. The sample totally broken, it does not seem that the failure occured due to weld defect. 

Regards,
Himan Nikdin

On Jan 25, 2019, at 08:44, Brijesh Maurya <brijeshmaurya492@gmail.com> wrote:

First you should do  the RT of sample to check if there is any defect in weld or not.

On Thu, Jan 24, 2019, 7:01 PM Himan Nikdin <himan.nikdin@outlook.com wrote:
Dear Experts

A PQR sample has been welded per below procedure;
SB-209 Grade 5183
THK; 40 mm
Process; GTAW
Filer metal; ER5183
Shielding gas; Argon
Preheat Temp; 70°C/Interpass Temp; 100°C
but all four bend samples rejected due to facture, meanwhile the tensile result is less than acceptable criteria.
would you please advise me in regards to the reason for this failure.

Thanks Indeed
Himan Nikdin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...