Re: [MW:28978] SB-209 Grade 5183-PQR failure

You proceed to another PQR sample and all tests without changing anything ...?
I wish I was the lab which does the tests for you.

Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Sat, Jan 26, 2019 at 10:43 AM Himan Nikdin <himan.nikdin@outlook.com> wrote:
RT done, some porosity observed, but in the acceptable critera per ASME IX. The sample totally broken, it does not seem that the failure occured due to weld defect. 

Regards,
Himan Nikdin

On Jan 25, 2019, at 08:44, Brijesh Maurya <brijeshmaurya492@gmail.com> wrote:

First you should do  the RT of sample to check if there is any defect in weld or not.

On Thu, Jan 24, 2019, 7:01 PM Himan Nikdin <himan.nikdin@outlook.com wrote:
Dear Experts

A PQR sample has been welded per below procedure;
SB-209 Grade 5183
THK; 40 mm
Process; GTAW
Filer metal; ER5183
Shielding gas; Argon
Preheat Temp; 70°C/Interpass Temp; 100°C
but all four bend samples rejected due to facture, meanwhile the tensile result is less than acceptable criteria.
would you please advise me in regards to the reason for this failure.

Thanks Indeed
Himan Nikdin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...