Hi,

It does't matter if the WPS has been approved by god himself...!!!
Approved or not, it seems that it is causing you problems.
It is impossible for a client to accept such defects, forget about it.
Do not waste your time and start your repairs. The way you are trying to resolve the issue is not going to work...

Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Tue, Jan 22, 2019 at 9:37 AM riaz rafeeque <riaz.rafeeque@gmail.com> wrote:
This is the wps approved. 


Backing with cupper shoes

On Sun, Jan 20, 2019, 11:34 AM Ramin Kondori <raminkondori@gmail.com wrote:
I read the comments.
Why don't you correct your welding procedure...?
All these discussions aside, finally your meat is under your client's teeth.
So I recommend you first to correct the issue. This way you will have more of your client support.
But if you don't and just try to justify, it will make them more upset. Believe me, I have been the client's inspector all my career.
Tell me about the welding procedure. 

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Wed, Jan 16, 2019 at 7:24 PM Ri@z <riaz.rafeeque@gmail.com> wrote:

Dear All,

Our Pipeline specification not accepting Incomplete Fusion .In case of incomplete fusion weld shall be rejected and re-welded.


But according to API 1104, IF and IFD are different . So is it required to reject both IF and IFD as both are incomplete Fusion?

Please help me with advice 


I am using AUT for the inspection and 70 % of joints are detecting either IF or IFD 




With Regards

Riaz 





Pls help me 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/lJ1fIfkP9Lc/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...