Hi,

Who told you to perform AUT? I mean why not RT? AUT will hold your project in Reverse gear.

Mostly in stringent case we perform AUT/PAUT/TOFD or where there is multiple requirement like tie-in's, anyhow it's mutual agreement between company and contractor.

And yes both are different by 9.3.4 / 9.3.5, ID and IFD, you cannot straight away reject but contemplate upon given para condition as per the pipe sizes then proceed for acceptance/rejections.

Thanks
Muneeb

On Wed, Jan 16, 2019, 9:24 PM Ri@z <riaz.rafeeque@gmail.com> wrote:

Dear All,

Our Pipeline specification not accepting Incomplete Fusion .In case of incomplete fusion weld shall be rejected and re-welded.


But according to API 1104, IF and IFD are different . So is it required to reject both IF and IFD as both are incomplete Fusion?

Please help me with advice 


I am using AUT for the inspection and 70 % of joints are detecting either IF or IFD 




With Regards

Riaz 





Pls help me 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...