[MW:28982] Backing gas as per API RP 582

Dear Experts,

As per clause 7.3 of API RP 582 Ed. 2016 back purging required for GTAW & GMAW process but no where I could found for other process like SMAW.  Is it mean that if we do welding with SMAW process back purging is not required?

Please share your interpretation.

Thanks and regards

Manoj.


--