Wednesday, January 16, 2019

[MW:28920] IF ans IFD as per API 1104


Dear All,

Our Pipeline specification not accepting Incomplete Fusion .In case of incomplete fusion weld shall be rejected and re-welded.


But according to API 1104, IF and IFD are different . So is it required to reject both IF and IFD as both are incomplete Fusion?

Please help me with advice 


I am using AUT for the inspection and 70 % of joints are detecting either IF or IFD 




With Regards

Riaz 





Pls help me 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...