Hi
Pl refer QW-350 for the essential variable for Welder.
QW-351 GENERAL " A welder shall be requalified whenever a change is made in one or more of the essential variables listed for each welding process."
WPQ is not only depend on P numbers, there are other variables are also to be considered.
Pl check your essential variable against your welding process.
Example For SMAW,
Change in base metal P no is essential variable, i.e. QW- 403.18
Thanks and Regards
Rameshkannan Devaraj
"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"
--On Sun, Nov 11, 2018 at 7:49 AM Surendra <skchordia.bhl@gmail.com> wrote:Hello,--I have individual qualified welders per BPVC Section-IX-2015, as per following detail:1. P1,G1 TO P1,G12. P8,G1 TO P8,G1Can I use the same welder for welding of following?1. P1,G1 TO P8,G1Thanking You,SurendraBhilwara, Rajastha(Ind)
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Monday, November 12, 2018
Re: Re: Re: Re: [MW:28618] Welder qualification
I have individual qualified welders per BPVC Section-IX-2015, as per following detail:
1. P1,G1 TO P1,G1
2. P8,G1 TO P8,G1
Can I use the same welder for welding of following?
1. P1,G1 TO P8,G1
REPLY:
Read QW-350 will describe you the most common factors affecting the essential variables of process like dimater, thickness, t weld depostions, main factors in your case listed as per below,
1) Approved procedure (WPS) for your dissimilar.
2) Should not be change in F-no (WPS vs WPQ-Performance) same F.
3) Should not omit inert gas backing on the job.
4) Lastly clarity on P1,G1 TO P1,G1 and P8,G1 TO P8,G1 qualified welder to P1,G1 TO P8,G1 disimilar, for this scenario both welders can weld as this scenario will not have omit in backing gas , with same F nos on job and as per QW-423 table.
5) Refer QW-350, 408.8, QW-423 and QW-433
Concluding that if your production ensured with all common and main factorts above, then yes you can.
Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2
AWS-CWI (2007)
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SA SAP#:70021650 JAPID, QCS & QCI.
M +91-636-955-7189 & +91-801-521-6854.
U r correct!
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Souravbohray
Sent: 12 November 2018 11:17
To: Materials & Welding
Subject: [MW:28616] Welder qualification
Can't use because change in P no Nd u dnt hv qualified for p8 to p1. You have only p1 to p1 and p8 to p8.
you have qualified cs to cs and as to ss.
But u dnt hv qualified ms to ss .it's different u cnt use .if I m wrong correct me.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Can't use because change in P no Nd u dnt hv qualified for p8 to p1. You have only p1 to p1 and p8 to p8.
you have qualified cs to cs and as to ss.
But u dnt hv qualified ms to ss .it's different u cnt use .if I m wrong correct me.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment