Thats great.

If the code of construction is B31.3, you follow the specific requirements for WPS impact qualification. If the requirements for impact qualification are more stringent than Section IX, so be it. Remember Section IX is a service code book and when a code of construction requires more stringent requirements, they must be followed. anyhow Check, B 31.3 Table 323.3.1 A5 and QW 403.6.

API 1104 and ASME IX have different mechanical testing requirements, as well as different requirements for testing equipment. You could use the same welding parameters and develop welding procedures that meet the requirements of each relevant code/specification, but the testing must meet the requirements of each relevant code/specification. In general, API 1104 will require more mechanical testing than will an ASME IX WPS, however, you cannot use the API 1104 test results to develop an ASME IX WPS for reasons stated above. 


Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

(6:59) He has the keys to the realm that lies beyond the reach of human perception; none knows them but He. And He knows what is on the land and in the sea; there is not a leaf which falls that He does not know about and there is not a grain in the darkness of the earth or anything green or dry which has not been recorded in a Clear Book.

 
Date: 2018-11-23 00:24
Subject: Re: [MW:28660] Impact requirement of multiple process and different Group number
What is the construction Code?
Pls note that Section IX does not deal with impact test at all

Στις Δευ, 19 Νοε 2018, 09:40 ο χρήστης Ri@z <riaz.rafeeque@gmail.com> έγραψε:
Dear All, 


PQR conducted on P1G1#p1G3 with wall thickness 7.8 mm. Root Hot Pass with GTAW and Remaining SMAW. 


1) Is this required to carry out impact test of HAZ for both G1 and G3 material ?

2) Is it required to carry out impact test for both GTAW and SMAW process separately ??


With Regards

Riaz  

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...