May be u looking for simple answer as below !

 

Thickness range qualified as per ASME Sec 9


Without impact  5 to 40 mm as per QW-451.1

With impact 16 to 40 mm as per QW- 403.6

 

Thickness range qualified as per ASME B31.3, Refer Chapter V, 328.2

Same as above


 

Shoot your queries in order to understand and respond properly by our team members 

Thanks for understanding 



Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Wed, Nov 14, 2018 at 6:30 PM muneebslsa@gmail.com <muneebslsa@gmail.com> wrote:
Yes its not clear.

If i am not wrong check Interpretation: IX-10-34, for your scenario.

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 & AWS-CWI
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

Say (O Muhammad SAW to mankind). "If the sea were ink for (writing) the Words of my Lord, surely, the sea would be exhausted before the Words of my Lord would be finished, even if we brought (another sea) like it for its aid."18-109

 
From: Paidi
Date: 2018-11-14 19:29
Subject: Re: [MW:28625] Thickness range for PQR
Jibin , 

Your Question is incomplete , please brief clearly your requirement . 

Suresh 

On Wed, Nov 14, 2018 at 3:44 PM Jibin Philip <jibinphilip123@gmail.com> wrote:
Dear Experts..

code asme sec 9 ,B31.3 .. pqr test plate thickness is 20 mm ..need charpy test .. so what will be thickness range qualified ??
Regards,
Jibin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Thanks  & Best Regards,

Suresh Paidi


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...