RE: [MW:28691] Re: Need Proof loads for SA-193

Hi Thaksen,

 

Please look at Sec-II, Part -D, Table-3, allowable stresses. There're many grades under this specification. Hence need to choose the correct grade for the appropriate allowable stress.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of chiluka venkatramulu
Sent: November 25, 2018 4:55 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:28690] Re: Need Proof loads for SA-193

 

Proof load is for Nuts I.e SA 194 only.

 

On Sun, 25 Nov 2018, 12:35 pm 'Thaksen Ingole' via Materials & Welding <materials-welding@googlegroups.com wrote:

Dear Member,

 

 

Does ASME Sec.II Part A list the proof loads for SA-193 material. I have seen the code but i couldn't find any values in SA-193 section. Could some one direct me to the page where these values are listed in this code.

 

Warm Regards

Thaksen Ingole

 

 

 

 

On Thursday, 1 November, 2018, 2:52:14 PM GMT+3, Thaksen Ingole <t_ingole@yahoo.co.in> wrote:

 

 

 

 

Dear Member,

 

 

Does ASME Sec.II Part A list the proof loads for SA-193 material. I have seen the code but i couldn't find any values in SA-193 section. Could some one direct me to the page where these values are listed in this code.

 

Warm Regards

Thaksen Ingole

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...