Re: [MW:28690] Re: Need Proof loads for SA-193

Proof load is for Nuts I.e SA 194 only.

On Sun, 25 Nov 2018, 12:35 pm 'Thaksen Ingole' via Materials & Welding <materials-welding@googlegroups.com wrote:
Dear Member,


Does ASME Sec.II Part A list the proof loads for SA-193 material. I have seen the code but i couldn't find any values in SA-193 section. Could some one direct me to the page where these values are listed in this code.

Warm Regards
Thaksen Ingole




On Thursday, 1 November, 2018, 2:52:14 PM GMT+3, Thaksen Ingole <t_ingole@yahoo.co.in> wrote:




Dear Member,


Does ASME Sec.II Part A list the proof loads for SA-193 material. I have seen the code but i couldn't find any values in SA-193 section. Could some one direct me to the page where these values are listed in this code.

Warm Regards
Thaksen Ingole

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...