Sunday, November 25, 2018

Re: [MW:28689] PQR for lining - SA516 GR 70 TO HASTALLOY C276

Dear dinesh,

Its possible to do PQR  for SA516 Gr.70 plate with Hastalloy C276. I would suggest ENiCrMo14 filler with GTAW process. Probably it would be a Lap fillet welding so take a SA516 Gr.70 plate and hastalloy C276 sheet and make a production mock up PQR and then do Macro as per ASME Sec IX.

It would qualify your purpose.
Cheers.

Regards,
G.jayaprakash.
Manufacturing Engineering Manager (welding). 


On Sun, 25 Nov 2018, 8:05 am Dinesh Somwanshi, <som.din@gmail.com> wrote:

Dear sir.

It will be welded on internal surface on Nozzle.

Thanking You,

With Regards..
Dinesh V Somwanshi
Api 570, Cswip 3.1,Bgas 2
Authorised Certified Piping, Welding, Painting Inspector.
00919881344135

On 24 Nov 2018 21:53, "pgoswami" <pgoswami@quickclic.net> wrote:
You should use consumable matching the chemistry& specification of hastelloy C276 for this dissimilar weld. 
Where this weld would apply, external support?
Please clarify. 
Thanks. 




Sent from my Bell Samsung device over Canada's largest network.

-------- Original message --------
From: Dinesh Somwanshi <som.din@gmail.com>
Date: 2018-11-24 07:22 (GMT-05:00)
Subject: [MW:28682] PQR for lining - SA516 GR 70 TO HASTALLOY C276

Dear sir,

Would possible to advice with PQR for lining - SA516 GR 70 TO HASTALLOY C276.

Please advice.


Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER

AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
 00919881344135 India 
Skype = dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...