If the initial PQR was done with filler metal classification without the letter G at the end you don't need a new PQR
Στις Παρ, 16 Νοε 2018, 07:45 ο χρήστης HARISH VARUDE <harish.varude02@gmail.com> έγραψε:
Dear All Expert.--With reference to the above subject,our contractor want to change electrode brand and manufacturer.So I would like to know should I need to create new Welding procedure again due to changes in electrode brand and manufacturer?Please let me know about this query.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments