Re: [MW:28646] Welder qualification thickness of API 1104

As per clauses 6.2.2.a.2 and 6.3.1 and 6.3.2.a.2 of API 1104, you do not have provision to qualify something what has been described below, because the consequences of ASME IX are different from API 1104 and it is more stringent.

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 & AWS-CWI (2007)
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

Say (O Muhammad SAW to mankind). "If the sea were ink for (writing) the Words of my Lord, surely, the sea would be exhausted before the Words of my Lord would be finished, even if we brought (another sea) like it for its aid."18-109

 
From: Ri@z
Date: 2018-11-16 12:59
Subject: [MW:28638] Welder qualification thickness of API 1104
Dear All,


i have deployed two welder for root-hotpass and filler-capping. 


thickness of joint is 6.6 mm.  Root- hotpass combined deposited thickness is 4 mm and remaining  2 mm thickness is fillled up with another welder.

Now how can I distribute the thickness qualification for different welders. 

Can I consider Nominal thickness for both welders ?

or Should i split thickness for both welders ??


Pls help 


With Regards

Ray

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...