Friday, November 16, 2018

Re: [MW:28638] Filler metal ER70S-G

Refer SFA 5.18 part C of SEC-2.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 & AWS-CWI (2007)
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

Say (O Muhammad SAW to mankind). "If the sea were ink for (writing) the Words of my Lord, surely, the sea would be exhausted before the Words of my Lord would be finished, even if we brought (another sea) like it for its aid."18-109

 
Date: 2018-11-15 23:03
Subject: [MW:28633] Filler metal ER70S-G

Dears experts.

Please can anyone helps me about the difference between ER70S-3 and ER70S-G.

Best regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...