Re: [MW:28633] ALLOY N08825 Welding and Testing requirements

Please find below Aramco specs,
SAES-W-014 : Weld overlays and welding of clad materials
SAES-W-016: Welding of Special CRA materials
SAES-W--019:Girth welding requirements for clad pipes
01-SAMSS-044: CRA clad pipe spools.
select your stuff from this list. if you have any specific testing or area to address, please let me know.
Regards
ABDUL MUNEER M
+966550216718 (KSA)
+919895480850 (IND)


On Thu, Nov 15, 2018 at 9:28 AM Ramesh <rameshkannandevaraj@gmail.com> wrote:
Members,

Pl share any reference for ALLOY N08825 Welding and Testing requirements in detail, especially looking for ARAMCO requirements ( reference numbers atleast )

Thank you in advance


Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...