refer this

QW-423 Alternate Base Materials for Welder
Qualification





regard
rajesh

On Sun, Nov 11, 2018 at 5:19 AM Surendra <skchordia.bhl@gmail.com> wrote:
Hello,

I have individual qualified welders per BPVC Section-IX-2015, as per following detail:

1. P1,G1 TO P1,G1

2. P8,G1 TO P8,G1

Can I use the same welder for welding of following?

1. P1,G1  TO P8,G1 

Thanking You,

Surendra
Bhilwara, Rajastha(Ind)


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...