Friday, November 16, 2018

[MW:28638] API 1104 Internal Clamp and External Clamp

Dear  All,


External clamp and internal clamp WPS and PQR procedures are qualified with downhill process and uphill process respectively.  But one joint has welded with internal clamp following  all other variables as of external clamp WPS


Is this acceptable ? If yes , how can we justify ?

Pls help very urgent 


Ray


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...