RE: [SOCIAL NETWORK] [MW:27825] Pressure test of heat exchanger having a PSV

Check the design pressure for which the heat exchanger has been rated. Maybe then you can decide whether 26bar pressure testing is required.

 

From: 'Asif Shahzad' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: Thursday, May 10, 2018 12:25 PM
To: Materials & Welding
Subject: [SOCIAL NETWORK] [MW:27821] Pressure test of heat exchanger having a PSV

 

Dear Expert,

 

We have heat exchanger that should be pressure tested at 26 Bar while at the piping attached with exchanger having a PSV set at 17 bar and we can not remove and isolate the PSV because of welding.

 

Can we limit the pressure test at 15 or 16 bar? .Plz provide your expert opinion.

 

Regards,

 

Asif 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...