Tuesday, May 29, 2018

Re: [MW:27921] Permissible dent on pipe

what is ref std pl 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Mon, May 28, 2018 at 10:27 PM, chandrakant mohikar <crmohikar@gmail.com> wrote:
Dent (buckling and or upheavel ) in piping shall be <2 %. In addition NDT shall be carried at dent location has to be as per requirement to ensure fitness of piping or RBI (Risk based inspection)

Chandrakant Mohikar
Ex. PDO / Co. Site Representative (Project QA)

8446079514


On Mon, 28 May 2018, 4:10 p.m. Anoj Singh, <nayaktp@gmail.com> wrote:
What is permissible dent on 10" sch. Std. Carbon steel seamless pipe?

Regards
Anoj singh


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...