Re: [MW:27915] PWHT in Sulphur Storage Tanks

Dear Friend
Sulphur iscorrosive element form Sulphides to reduce the intensity of corrosion one must control its hardness below 185BHN or say as per NACE 
Therefore for NACE  application PWHT is essential Most of the time SA516 Gr 60 is recomended for CS eqpt
Regards
Hegde

On Friday, 25 May, 2018, 5:06:18 PM IST, pkkanishk2006@gmail.com <pkkanishk2006@gmail.com> wrote:


Dear Experts ,

Please can anyone help me to understand the requirement of PWHT in Sulphur Storage tankages . Is it normally needed ? Is anything else we have to look for other than thickness and Material Composition ? 


Kindly help with more details if i missed anything 

Regards,
Anand

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...