Monday, May 28, 2018

Re: [MW:27914] Permissible dent on pipe

Dear Anoj,

You will not find the straight answer for this question.
First you have to visually check the size (depth, length, width), sharpness and if the shape of the pipe has been changed. Based on these observations you can decide if further investigation has to be done like measurement of thickness reduction, NDT to find if any surface and/or internal defects are developed. If above tests, measurements, shape are acceptable, pipe can be used.

Thanks,
Warm Regards,

Rajnish Dixit
Lead - QA-QC/QMS/Welding/NDT/Inspection
+91 972 4200 357

On Mon, May 28, 2018 at 16:10, Anoj Singh
<nayaktp@gmail.com> wrote:
What is permissible dent on 10" sch. Std. Carbon steel seamless pipe?

Regards
Anoj singh


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...