Yes, can.
Follow API 653 requirments.
On Sat, May 26, 2018, 8:58 AM 'Neilash Kumar' via Materials & Welding <materials-welding@googlegroups.com> wrote:
--Hi ,You need to replace the full bottom plate in order to avoid the further breakdown during service.NeilashkumarOn Saturday, 26 May, 2018, 5:59:46 AM GMT+3, Shanmugam <nss2410@gmail.com> wrote:--Dear Experts,During sutdown after blasting tank bottom plates we observed lot of pitting corrosion. Some pitting are went through the entire thickness and some pittings are in the half way of the thickness.By following API 653 is it possible to repair with patch plate on the holes formed and went through the entire bottom plate thickness by pitting corrosion. Your kind suggestion is requested.Tank Construction code: API -650Bottom plate thickness - 8mm
With Regards,
N.S
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments