Wednesday, May 16, 2018

RE: [MW:27851] Under Water welding

Hello peers,

Can someone please advise on this? A sample WPS can work too.

Thanks in advance and  looking for your kind advise.

 

 

With best regards,

Firoz Ahmed (Umar)


Op 10 mei 2018 om 23:38 heeft Umar <firoz.makrani@gmail.com> het volgende geschreven:

Dear Experts

I want to create a WPS for Underwater welding. The material is Structural steel welding repairs by patch. The environment is marine environment.

Could someone please provide me the information like process, filler material, welding perameters etc.

Thanks in advance for your kind support.

 

 

With best regards,

Firoz Ahmed (Umar)

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...