Tuesday, May 15, 2018

Re: [MW:27847] Re: If a welder is qualified with SS (Stainless Steel) GTAW, He can weld CS Carbon steel GTAW?

provided all other essential variable in order on process wise?

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sun, May 13, 2018 at 8:48 AM, Mohan <ggnanamalli@gmail.com> wrote:
HI Srinivas,

Pl find the below table extract from ASME Sec.IX QW-20 Base Metal Grouping,  if you qualified any one group P-1 to P-15F means he can weld upto P1- to P15F grouping metals




On Sat, May 12, 2018 at 11:21 AM, srinivas <SrinivasDuraisamy@gmail.com> wrote:

Hi , 

I have welder qualification P4 to P4 material. He can weld P5A materials ?. Plz give some reference though ASME  

Thanks,
Srinivas. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...